Heng, C. L.; Zalloum, O. H. Y.; Roschuk, T.; Blakie, D.; Wojcik, J.; Mascher, P.
(Electrochemical and Solid-State Letters,, 2007-05-02)
We have studied photoluminescence PL from samples of Er-doped Si-rich silicon oxide SRSO annealed at 875°C for 1 h in N2,
N2 + 5% H2 FG1, Ar + 5% H2 FG2, and O2, respectively, or subjected to double-step annealing processes. ...